Short drying time for the solid clay left considerable moisture remaining. The result was serious spalling and cracking of the clay slabs, particularly at the top of the smelter. Previous ![]() ![]() Text © Darrell Markewitz, 2017 Photographs © Darrell Markewitz, 2017 Copyright details Contact us |